复合硅源制备SiO 2气凝胶复合材料的性能研究
王蒙蒙, 刘红花, 李占峰, 王艳艳, 刘瑞祥, 孙传庆
Preparation and performance of SiO 2 aerogel composite materials using composite silicon source
Wang Mengmeng, Liu Honghua, Li Zhanfeng, Wang Yanyan, Liu Ruixiang, Sun Chuanqin
耐火材料 . 2026, (4): 338 -342 .  DOI: 10.3969/j.issn.1001-1935.2026.04.011