锆英石对矾土基莫来石均质料烧结行为及抗碱侵蚀性的影响
赵飞, 李若茜, 王亚利, 麦海香, 左玉冬, 安建成, 连伟康
Effect of zircon on sintering behavior and alkali corrosion resistance of bauxite-based mullite homogeneous grogs
Zhao Fei, Li Ruoxi, Wang Yali, Mai Haixiang, Zuo Yudong, An Jiancheng, Lian Weikang
耐火材料 . 2026, (5): 376 -382 .  DOI: 10.3969/j.issn.1001-1935.2026.05.002