镁锆粉对刚玉-尖晶石质浇注料性能的影响
雷宇湉, 聂建华, 陈瑞峰, 张小旭, 梁永和
Effect of magnesia-zirconia powder on properties of corundum-spinel based castables
Lei Yutian, Nie Jianhua, Chen Ruifeng, Zhang Xiaoxu, Liang Yonghe
耐火材料
.
2026, (5): 397
-401
.
DOI: 10.3969/j.issn.1001-1935.2026.05.005