精炼钢包用快烘防爆型复相刚玉-尖晶石浇注料的应用研究
胡波, 刘光平, 陈俊峰, 宋雅楠, 李媛媛, 王玉龙, 沈明科
Application of fast-baking and explosive-spalling-resistant composite corundum-spinel castables for refining ladles
Hu Bo, Liu Guangping, Chen Junfeng, Song Yanan, Li Yuanyuan, Wang Yulong, Shen Mingke
耐火材料
.
2026, (5): 408
-414
.
DOI: 10.3969/j.issn.1001-1935.2026.05.007