碳纳米纤维/铝酸钙复合粉对陶瓷复合电阻性能的影响
钟振鑫, 姚聪伟, 王云龙, 朱锐锋, 王佳一, 种小川, 肖国庆, 丁冬海
Effect of carbon nanofiber/calcium aluminate composite powder on properties of ceramic composite resistors
Zhong Zhenxin, Yao Congwei, Wang Yunlong, Zhu Ruifeng, Wang Jiayi, Chong Xiaochuan, Xiao Guoqing, Ding Donghai
耐火材料
.
2026, (5): 415
-421
.
DOI: 10.3969/j.issn.1001-1935.2026.05.008