危废处置回转窑用典型耐火材料抗熔渣侵蚀性能研究
易帅, 邓丽娜, 许谦, 司国栋, 陈美娜, 薛飞, 曾鲁举, 谢金莉
Slag corrosion resistance of typical refractories for rotary kilns of hazardous waste disposal industry
Yi Shuai, Deng Lina, Xu Qian, Si Guodong, Chen Meina, Xue Fei, Zeng Luju, Xie Jinli
耐火材料
.
2021, (2): 121
-125
.
DOI: 10.3969/j.issn.1001-1935.2021.02.007