南钢电弧炉炼钢烟尘沉降室用耐火材料抗侵蚀性研究
李权辉, 于建宾, 李翔, 马渭奎
Corrosion resistance of the refractories used in the soot settling chamber of Nangang EAF steelmaking
Li Quanhui, Yu Jianbin, Li Xiang, Ma Weikui
耐火材料 . 2021, (1): 73 -76 .  DOI: 10.3969/j.issn.1001-1935.2021.01.016