Refractories ›› 2025, Vol. 59 ›› Issue (5): 369-374.DOI: 10.3969/j.issn.1001-1935.2025.05.001

    Next Articles

Interfacial reactions of nitrogen-based refractories with lanthanum oxide and lanthanum aluminate

Ma Fei-xiang, Li Hongxia, Liu Guoqi, Gu Qiang   

  1. First author's address:School of Materials Science and Engineering,Henan University of Science and Technology,Luoyang 471003,Henan,China
  • Received:2025-01-03 Online:2025-10-15 Published:2025-10-22

氮基耐火材料与氧化镧和铝酸镧的界面反应研究

马飞祥1,2), 李红霞1,2), 刘国齐2), 顾强2)   

  1. 1)河南科技大学 材料科学与工程学院 河南洛阳 471003
    2)中钢集团洛阳耐火材料研究院有限公司 先进耐火材料全国重点实验室 河南洛阳 471039
  • 作者简介:马飞祥:男,1995年生,博士研究生。E-mail:2537245145@qq.com
  • 基金资助:
    国家青年科学基金项目(52302031);国家自然科学基金项目(51932008, 51772277);华中千人工程(204200510011)。

Abstract: To develop specific lining materials for rare earth steel nozzles,LaAlO3 powder was first synthesized by high-temperature solid-phase synthesis at 1 400 ℃ for 3 h using La2O3 and Al2O3 powders as raw materials.Then BN,AlN,Si3N4 and TiN powders were pressed into Φ30 mm×7 mm substrate samples with PVA as the binder under 120 MPa.Equal amounts of La2O3 and LaAlO3 powders were placed on their surfaces,reacting at 1 550 ℃ for 3 h in different atmospheres (reducing and argon conditions).The interfacial reactions of the four nitride (BN,Si3N4,AlN,and TiN) substrate samples with La2O3 and LaAlO3 in different atmospheres were studied,respectively.The results show that in reducing and argon atmospheres,the intensity order of the reactions between the four nitrides and La2O3 is Si3N4>BN>AlN>TiN.In the reducing atmosphere,the reaction intensity order of the four nitrides with LaAlO3 is Si3N4>AlN≈TiN>BN.However,in the argon atmosphere,the order is Si3N4>BN>AlN≈TiN.TiN has good structural stability in both reducing and argon atmospheres,and reacts slightly with La2O3 and LaAlO3.It is a relatively good anti-clogging lining material for rare earth steel nozzles.

Key words: nitride-based refractories, interfacial reaction, rare earth steel, anti-clogging lining

摘要: 为开发稀土钢专用水口内衬材料,首先以La2O3和Al2O3粉为原料,于1 400 ℃保温3 h高温固相合成LaAlO3粉体;再分别将BN、AlN、Si3N4、TiN粉体以PVA为结合剂在120 MPa压力下压制成Φ30 mm×7 mm的衬底试样,在其表面分别放置等量的La2O3和LaAlO3粉,在还原和氩气气氛条件下于1 550 ℃反应3 h。研究了4种氮化物(BN、Si3N4、AlN、TiN)衬底试样分别与La2O3和LaAlO3在还原和氩气气氛条件下的界面反应。结果表明:在还原和氩气气氛下,4种氮化物与La2O3反应的强弱顺序皆是Si3N4>BN>AlN>TiN;在还原气氛下,4种氮化物与LaAlO3反应的强弱顺序是Si3N4>AlN≈TiN>BN,但在氩气气氛下,其反应顺序是Si3N4>BN>AlN≈TiN;TiN在还原和氩气气氛下均具有较好的结构稳定性,与La2O3、LaAlO3反应较弱,是一种较好的稀土钢水口防堵内衬材料。

关键词: 氮基耐火材料, 界面反应, 稀土钢, 防堵内衬