Preparation process of water based tape casting of plate-like silicon nitride ceramics
Zhao Chenxiao, Li Shipeng, Wang Gang, Yuan Bo
First author's address:State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
Zhao Chenxiao, Li Shipeng, Wang Gang, Yuan Bo. Preparation process of water based tape casting of plate-like silicon nitride ceramics[J]. Refractories, 2025, 59(5): 427-431.
[1] 董其政.环保非水基流延成型制备高质量氧化锆陶瓷基片及氮化硅生坯的研究[D].景德镇:景德镇陶瓷大学,2018. [2] 余冬玲,张会玲,罗宏斌,等.MgO和Y2O3对气压烧结制备氮化硅陶瓷的影响[J].耐火材料,2021,55(4):316-318. [3] 周玉栋,李世鹏,王文武,等.高导热氮化硅陶瓷的制备研究进展[J].耐火材料,2024,58(3):270-276. [4] 赵辰啸,李世鹏,王刚,等.流延成型技术制备片状氮化硅陶瓷研究进展[J].耐火材料,2025,59(2):177-184. [5] 张云龙,张宇民,赵晓静,等.湿法成形陶瓷料浆研究进展[J].兵器材料科学与工程,2007,30(1):66-71. [6] 赵芃,谢光远,宗红军,等.氧化锆PVA-水基流延成型工艺研究[J].硅酸盐通报,2016,35(10):3336-3339. [7] 付杰,刘源,赵振威,等.Y2O3-MgO外加量对Isobam凝胶流延氮化硅性能的影响[J].耐火材料,2024,58(5):400-404. [8] 昝青峰,黄勇,汪长安,等.流延法在Si3N4块体及Si3N4/BN层状材料制备中的应用[J].佛山陶瓷,2001,11(11):6-9. [9] LIU S C,YE F,LIU L M,et al.Feasibility of preparing of silicon nitride ceramics components by aqueous tape casting in combination with laminated object manufacturing[J].Materials & Design,2015,66:331-335. [10] REN L C,LUO X F,ZHOU H Q.The tape casting process for manufacturing low-temperature co-fired ceramic green sheets:A review[J].Journal of the American Ceramic Society,2018,101(9):3874-3889. [11] 黄智勇,王翔,刘学建,等.氮化硅粉体的行星式球磨工艺研究[J].陶瓷科学与艺术,2003,37(6):21-25. [12] 谢雨洲,彭超群,王小锋,等.流延成型技术的研究进展[J].中国有色金属学报,2015,25(7):1846-1857.