Preparation and properties of porous MgAl2O4 ceramics by low-temperature combustion

Piao Jiasi, Du Qingyang, Bai Jiahai   

  1. School of Materials Science and Engineering,Shandong University of Technology,Zibo 255049,Shandong,China
  • Received:2021-11-03 Online:2022-08-15 Published:2022-11-09

低温燃烧合成MgAl2O4多孔陶瓷及其性能研究

朴佳思, 杜庆洋, 白佳海   

  1. 山东理工大学 材料科学与工程学院 山东淄博 255049
  • 通讯作者: 白佳海,男,1971年生,博士,副教授。E-mail:287694198@qq.com
  • 作者简介:朴佳思:女,1997年生,硕士研究生。E-mail:1597180588@qq.com
  • 基金资助:
    山东省自然科学基金项目(ZR2019MEM045)。

Abstract: To lower the synthesis temperature of MgAl2O4 and the energy consumption,MgAl2O4 powders were synthesized via a low-temperature combustion route using Al(NO3)3·9H2O,Mg(NO3)2·6H2O and NH4NO3 as oxidizing agents,C2H5NO2 and CH4N2O as reducing agents,and EDTA as the fuel.Then porous MgAl2O4 ceramics were prepared with the prepared powders or the prepared powders treated at 800 ℃.The effects of the EDTA addition (0,2.5%,5%,7.5% of the reducing agents,by mole) on the properties of the MgAl2O4 powders and the porous MgAl2O4 ceramics were studied.The experimental results show that:(1)with the increase of the EDTA addition in the precursors,the ignition loss increases and the specific surface area of the MgAl2O4 powders rises significantly;(2) with the increase of the EDTA addition in the precursors,the water absorption and the apparent porosity of the porous MgAl2O4 ceramics obviously decrease,the bulk density increases significantly,and the grain size of MgAl2O4 decreases slightly;(3)compared with the ceramics prepared from the MgAl2O4 powders treated at 800 ℃,the porous MgAl2O4 ceramics prepared with the MgAl2O4 powders have relatively higher water absorption and apparent porosity,and more uniform microstructure;(4)when the EDTA addition is 2.5% of the reducing agents,the porous ceramic sample prepared with the MgAl2O4 powders has the water absorption of 23.8%,the apparent porosity of 46.9%,and the bulk density of 1.9 g·cm-3,presenting uniform microstructure.

Key words: low-temperature combustion, MgAl2O4 powder, porous MgAl2O4 ceramics, apparent porosity, microstructure

摘要: 为降低MgAl2O4的合成温度,减少能耗,以硝酸铝、硝酸镁和硝酸铵作为氧化剂,甘氨酸、尿素(CH4N2O)作为还原剂,乙二胺四乙酸(EDTA)为燃料,低温燃烧合成MgAl2O4粉体,并分别用该粉体和800 ℃处理后粉体制备了MgAl2O4多孔陶瓷。研究了EDTA加入量(分别为还原剂物质的量的0、2.5%、5%、7.5%)对MgAl2O4粉体及其多孔陶瓷性能的影响。结果表明:1)随EDTA加入量的增大,MgAl2O4粉体的烧失率增加,比表面积显著增大;2)随EDTA加入量的增大,MgAl2O4多孔陶瓷的吸水率和显气孔率显著降低,体积密度明显增加,MgAl2O4晶粒尺寸有所减小;3)与800 ℃处理后MgAl2O4粉体相比,用未处理的合成MgAl2O4粉体制备的多孔陶瓷的吸水率和显气孔率相对较高,显微结构较均匀;4)当EDTA加入量为还原剂的2.5%(x)时,以未处理的合成MgAl2O4粉体制备的多孔陶瓷的吸水率为23.8%,显气孔率为46.9%,体积密度为1.9 g·cm-3,显微结构较均匀。