Refractories ›› 2022, Vol. 56 ›› Issue (6): 499-504.DOI: 10.3969/j.issn.1001-1935.2022.06.009

Previous Articles     Next Articles

Influence of alumina-rich spinel micropowder on key performances of corundum-spinel castables

Xiao Xiong, Wei Yaowu, Zhou Hui, Yan Lin, Chen Zhiqiang, Shao Changbo   

  1. School of Materials and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2022-01-26 Online:2022-12-15 Published:2022-12-26

富铝尖晶石微粉对刚玉-尖晶石浇注料关键使用性能的影响

肖雄1), 魏耀武1), 周辉2), 颜林3), 陈志强3), 邵长波3)   

  1. 1)武汉科技大学 材料与冶金学院 湖北武汉 430081
    2)武汉钢铁集团耐火材料有限责任公司 湖北武汉 430082
    3)山东恒嘉高纯铝业科技股份有限公司 山东邹平 256220
  • 通讯作者: 魏耀武,男,1969年生,教授。E-mail:weiyaowu@wust.edu.cn
  • 作者简介:肖雄:男,1996年生,硕士研究生。E-mail:2376259628@qq.com

Abstract: The study aims to research the influence of alumina-rich spinel micropowders with different alumina contents on the key performances of corundum-spinel castables.The corundum-spinel castables were prepared using tabular corundum particles (6-3,3-1,≤1 mm) and spinel particles (≤1 mm) as the aggregates,tabular corundum fines (≤0.074 mm),spinel fines (≤0.032 mm ),active α-Al2O3 micropowder (d90=10.0 μm) and magnesium aluminate spinel micropowders with different alumina contents as the fine powder,Secar 71 cement as the binder.The mass ratio of aggregates to fines was 66.5∶33.5.Fixing the addition of alumina-rich spinel micropowders at 7 mass%,the effects on the microstructure and the key performances of the corundum-spinel castables were studied.The results show that:(1)the addition of aluminum-rich spinel micropowder is helpful to improve the hot modulus of rupture,the thermal shock resistance,and the slag resistance of the castables;a large amount of calcium hexaluminate forms and uniformly distributes on the slag-castables boundaries,hindering the penetration of ladle refining slag to the castables;(2)when the alumina content in alumina-rich spinel micropowder is 90%,the developed sample has good slag penetration resistance.

Key words: magnesium aluminate spinel, corundum-spinel castables, slag resistance, thermal shock resistance

摘要: 为研究不同氧化铝含量的富铝尖晶石微粉对刚玉-尖晶石浇注料关键使用性能的影响,以粒度为6~3、3~1和≤1 mm的板状刚玉颗粒和≤1 mm的尖晶石颗粒为骨料,以≤0.074 mm的板状刚玉细粉、≤0.032 mm的尖晶石细粉、d90=10.0 μm的活性α-Al2O3微粉和不同氧化铝含量的镁铝尖晶石微粉为细粉,Secar 71水泥为结合剂,按骨料与粉料质量比为66.5∶33.5进行配料,制备了刚玉-尖晶石浇注料。研究了不同氧化铝含量的富铝尖晶石微粉加入量为7%(w)时,对刚玉-尖晶石浇注料显微结构和关键使用性能的影响。结果表明:1)添加富铝尖晶石微粉有利于提高浇注料的高温抗折强度、抗热震性和抗渣性,且其可在渣-浇注料反应界面形成数量多且分布均匀的六铝酸钙,阻碍了钢包精炼渣在浇注料中的渗透。2)当富铝尖晶石微粉中氧化铝含量为90%(w)时,所制备的浇注料试样抗渣渗透能力较强。

关键词: 镁铝尖晶石, 刚玉-尖晶石浇注料, 抗渣性, 抗热震性