Refractories ›› 2023, Vol. 57 ›› Issue (1): 87-92.DOI: 10.3969/j.issn.1001-1935.2023.01.019

Previous Articles    

Research progress on oxidation behavior of SiAlON-based materials

Chen Xiaoyu, Feng Desheng, Wang Ye, Ouyang Deze, Liu Xinhong   

  1. School of Materials Science and Engineering,Zhengzhou University of Aeronautics,Zhengzhou 450046,Henan,China
  • Received:2022-02-24 Online:2023-02-15 Published:2023-02-21

SiAlON质材料氧化行为研究进展

陈晓雨1), 冯德胜1), 王晔2), 欧阳德泽2), 刘新红2)   

  1. 1)郑州航空工业管理学院 材料学院 河南郑州 450046
    2)郑州大学 河南省高温功能材料重点实验室 河南郑州 450052
  • 作者简介:陈晓雨:女,1993年生,硕士,助理实验师。E-mail:1160542658@qq.com

Abstract: The influences of the oxidation temperature,the oxidation time,the impurities,the particle size and the additive type on the oxidation behavior of SiAlON-based materials in China and abroad were summarized.It was pointed out that each factor had obvious effects on the phase composition,the microstructure,and the oxidation rate of the oxidation products,expecting to provide references for improving the service life of SiAlON-based materials.The future research direction was also indicated.

Key words: SiAlON-based materials, oxidation behavior, anti-oxidation

摘要: 综述了国内外关于氧化温度、氧化时间、杂质、粒度及添加剂种类等因素对SiAlON质材料氧化行为的影响,指出各因素对材料氧化产物物相组成、显微结构及氧化速率等有较明显的影响,期望为SiAlON质材料使用寿命的提高提供参考,同时指明将来研究方向。

关键词: SiAlON质材料, 氧化行为, 防氧化