Refractories ›› 2023, Vol. 57 ›› Issue (2): 169-174.DOI: 10.3969/j.issn.1001-1935.2023.02.018
Previous Articles Next Articles
Li Tao, Li Yage, Wu Shuai-bing, Li Hang, Lyu Junyi, Zhang Haijun
Received:2022-06-08
Online:2023-04-15
Published:2023-04-17
李韬, 李亚格, 吴帅兵, 李杭, 吕俊毅, 张海军
通讯作者:
张海军,男,1970年生,博士,教授。E-mail:zhanghaijun@wust.edu.cn
作者简介:李韬:男,1999年生,硕士研究生。E-mail:lt18339199818@163.com
基金资助:CLC Number:
Li Tao, Li Yage, Wu Shuai-bing, Li Hang, Lyu Junyi, Zhang Haijun. Research progress on boron-based antioxidants for carbon-containing refractories[J]. Refractories, 2023, 57(2): 169-174.
李韬, 李亚格, 吴帅兵, 李杭, 吕俊毅, 张海军. 含碳耐火材料用硼基抗氧化剂研究进展[J]. 耐火材料, 2023, 57(2): 169-174.
Add to citation manager EndNote|Ris|BibTeX
URL: http://www.nhcl.cn/EN/10.3969/j.issn.1001-1935.2023.02.018
| [1] 程贺朋,李红霞,杨彬,等.碳复合耐火材料对熔钢增碳作用的研究进展[J].中国冶金,2007,17(3):1-4. [2] 丁冬海,杨少雨,肖国庆.含碳耐火材料酚醛树脂结合剂的研究现状与展望[J].材料导报,2017,31(11):95-100. [3] 高陟,潘磊,马北越,等.铝碳耐火材料力学性能优化研究进展[J].钢铁研究学报,2022,34(1):27-34. [4] LI Y G,WANG J K,DUAN H J,et al.Catalytic preparation of carbon nanotube/SiC whisker bonded low carbon MgO-C refractories and their high-temperature mechanical properties[J].Ceramics International,2022,48(4):5546-5556. [5] 陈洋,邓承继,余超,等.镁钙碳耐火材料的研究进展[J].中国陶瓷工业,2018,25(2):15-19. [6] 张艳利,王宪,贾全利.炼钢转炉用耐火材料新技术现状及发展趋势[J].耐火与石灰,2021,46(2):1-8+14. [7] 徐平坤.炼钢转炉用耐火材料的技术进步[J].工业炉,2021,43(5):22-25+29. [8] 郭强.实现转炉出钢口长寿命的设想及措施[J].山东冶金,2021,43(3):14-15+18. [9] 蔡长秀,雷中兴,徐小峰,等.高性能转炉出钢口管砖的开发与应用[J].耐火材料,2021,55(4):325-328. [10] 彭小艳,李林,彭达岩,等.低碳镁炭砖及其研究进展[J].耐火材料,2003,37(6):355-357. [11] PILLI V,SARKAR R.Study on the nanocarbon containing Al2O3-C continuous casting refractories with reduced fixed carbon content[J].Journal of Alloys and Compounds,2019,781:149-158. [12] CHENG Y,ZHU T B,LI Y W,et al.Microstructure and properties of MgO-C refractory with different carbon contents[J].Ceramics International,2021,47(2):2538-2546. [13] LIU Z Y,YU J K,YANG X,et al.Oxidation resistance and wetting behavior of MgO-C refractories:effect of carbon content[J].Materials,2018,11(6):883. [14] 朱天彬,李亚伟,桑绍柏.低碳化镁碳耐火材料的研究进展[J].中国材料进展,2020,39(Z1):609-617. [15] 李红霞.双碳背景下耐火材料科技创新的思考[J].耐火材料,2021,55(5):381-384. [16] 于凌月,魏军从,杨春,等.不同碳源对低碳镁碳砖性能的影响[J].耐火材料,2020,54(4):338-342. [17] GOKCE A S,GURCAN C,OZGEN S,et al.The effect of antioxidants on the oxidation behaviour of magnesia-carbon refractory bricks[J].Ceramics International,2006,34(2):323-330. [18] LUZ A P,PANDOLFELLI V C.Artigo reviso:atuao dos antioxidantes em refratários contendo carbono[J].Cermica,2007,53(328):334-344. [19] ZHANG S,MARRIOTT N J,LEE W E.Thermochemistry and microstructures of MgO-C refractories containing various antioxidants[J].Journal of the European Ceramic Society,2001,21(8):1037-1047. [20] 高正霞,陶梦雅,刘伟,等.Al粉、Si粉复合低碳稳定镁钙材料的抗氧化性[J].耐火材料,2021,55(5):430-434. [21] HAYASHI S,TAKANAGE S,TAKAHASHI H,et al.Behaviour of boric compounds added in MgO-C bricks[J].Taikabutsu Overseas,1991,11(3):12-19. [22] YAMAGUCHI A.Self-repairing function in the carbon-containing refractory[J].International Journal of Applied Ceramic Technology,2007,4(6):490-495. [23] 高陟,马北越.低碳MgO-C耐火材料性能优化研究进展[J].钢铁研究学报,2021,33(5):353-362. [24] 陶强,马帅领,崔田,等.过渡金属硼化物的结构与性质[J].物理学报,2017,66(3):85-99. [25] 花桐誠司.転炉用 MgO-C れんがへの金属と CaB6 添加の併用効果[J].耐火物,1992,44(9):490-498. [26] 宋玉龙,陈敏.添加硼化钙对镁钙碳耐火材料抗氧化性能的影响[J].工业加热,2011,40(5):40-42. [27] 张连进,王义龙,张宏进,等.硼化钙加入量对Al2O3-SiC-C铁沟浇注料性能的影响[J].耐火材料,2016,50(1):60-63. [28] XU H,WANG X T,ZHANG W L,et al.The rapid synthesis of CaB6 powders by combining induction heating with carbothermic reduction and their antioxidant properties[J].Journal of the Australian Ceramic Society,2021,57(3):919-926. [29] 叶方保,钟香崇,MICHEL R.含硼添加剂对白云石碳和镁白云石碳材料热态强度的影响[J].耐火材料,2002,36(2):70-73. [30] 叶方保,钟香崇.含硼添加剂对白云石炭耐火材料抗氧化与抗侵蚀性的影响[J].耐火材料,1999,33(2):61-66. [31] 贺智勇,彭小艳,李林,等.ZrB2对低碳镁碳材料抗氧化性能的影响[J].耐火材料,2006,40 (4):280-282. [32] LI L,HONG Y R,SUN J L,et al.Formation of ZrB2 in MgO-C composite materials using in-situ synthesis method[J].Journal of Iron and Steel Research International,2006,13(1):70-74. [33] 李蕊,肖国庆,王浩.炭黑及ZrB2对低碳MgO-C耐火材料抗氧化性及显微结构的影响[J].硅酸盐通报,2013,32(4):738-742. [34] 姜乐,张连进,于凌月,等.ZrB2加入量对ASC铁沟浇注料性能的影响[J].耐火材料,2017,51(3):219-221. [35] 刘波,刘永锋,刘开琪,等.B4C对低碳MgO-C材料性能的影响[J].耐火材料,2010,44(1):14-16. [36] 遇龙,罗旭东,张国栋,等.BN对镁基含碳耐火材料性能的影响[J].人工晶体学报,2015,44(1):227-232,242. [37] 黄健,韩兵强,鄢文,等.BN粉加入量对Al2O3-SiC-C浇注料性能的影响[J].耐火材料,2019,53(5):354-358. [38] 连进,肖国庆,吕李华,等.添加MgB2对镁碳耐火材料抗氧化性能的影响[J].硅酸盐通报,2011,30(4):869-874. [39] 朱强,于景坤.添加LaB6对低碳镁碳砖抗氧化性能的影响[C]//全国博士生学术论坛——冶金工程分论坛,沈阳,2006:173-175. [40] WANG T,YAMAGUCHI A.Antioxidation behavior and effect of Al8B4C7 added to carbon containing refractories[J].Journal of the Ceramic Society of Japan,2000,108(1261):818-822. [41] LIU Y Q,JIANG Z,JIANG X,et al.New refractory MAB phases and their 2D derivatives:insight into the effects of valence electron concentration and chemical composition[J].RSC Advances,2020,10(43):25836-25847. [42] BAGHERABADI H M,NAGHIZADEH R,REZAIE H R,et al.The effects of aluminum and aluminum borate addition on the properties of MgO-C refractories[J].Journal of the Australian Ceramic Society,2019,55(1):281-288. [43] BAGHERABADI H M,NAGHIZADEH R,REZAIE H R, et al.Synthesis of dehydrated magnesium borate powders and the effect on the properties of MgO-C refractories[J].Journal of Ceramic Processing Research,2018,19(3):218-223. [44] 王志强,朱伯铨,方斌祥,等.B4C和Si组合抗氧化剂对低碳MgO-C砖抗氧化性能的影响[J].耐火材料,2008,42(3):161-164. [45] DING D H,CHONG X C,XIAO G Q,et al.Combustion synthesis of B4C/Al2O3/C composite powders and their effects on properties of low carbon MgO-C refractories[J].Ceramics International,2019,45(13):16433-16441. [46] 杨潘.含AlB2复合粉的燃烧合成及对低碳耐火材料抗氧化性能的影响[D].西安:西安建筑科技大学,2019. [47] CAMPOS K S,SILVA G,NUNES E H M,et al.The influence of B4C and MgB2 additions on the behavior of MgO-C bricks[J].Ceramics International,2012,38(7):5661-5667. [48] 宋玉龙.CaB6和B4C添加对MgO-CaO-C耐火材料抗氧化性影响的研究[D].沈阳:东北大学,2008. [49] 许欢.感应加热合成硼化物粉体及其在碳复合耐火材料中的作用[D].武汉:武汉科技大学,2018. [50] 刘贺,朱凌,李小超,等.添加锆英石、B4C和焦粉对铝碳质耐火材料抗氧化性能影响[J].人工晶体学报,2017,46(5):880-884+889. |
| [1] | Yao Luyan, Han Bingqiang, Zhang Jinhua, Ke Changming. Effect of Ti-Si-Fe alloy addition on structure and properties of Si3N4 bonded SiC refractories [J]. Refractories, 2024, 58(4): 277-283. |
| [2] | Zan Wenyu, Ma Beiyue, Chen Guangxin, Cao Changkun, Li Mengqiang. Preparation of porous mullite ceramic-based aggregates from low-voltage electroceramic wastes and secondary aluminum dross [J]. Refractories, 2024, 58(4): 302-306. |
| [3] | Deng Jiang, Liu Xuexin, Li Wen, Zhang Ziyi, Yuan Wenjie. Effects of alumina particle size and zirconia powder extra-addition on sintering property of alumina granulated powder [J]. Refractories, 2024, 58(4): 307-313. |
| [4] | Li Wenfeng, Shen Tianzi, Guo Huishi, Cao Jinjin, Kang Xiaoxu, Shi Kai, Kang Xiaoyang. Influence of polyhydroxy saccharide binders on properties of Al2O3-SiC-C waterless taphole clay [J]. Refractories, 2024, 58(4): 314-318. |
| [5] | An Jiarui, Zhang Rui, Fan Bingbing, Wang Gang, Du Penghui. Effects of Sm2O3 addition and heat treatment temperature on properties of CA6-MA materials [J]. Refractories, 2024, 58(4): 319-322. |
| [6] | Li Ying, Wang Di, Zhao Li, Yin Yicheng, Jia Quanli. Effect of graphite type on properties of Al2O3-MgO castables [J]. Refractories, 2024, 58(4): 323-328. |
| [7] | Ling Xiaxia, Xiang Yubo, Zheng Han, Wu Jiguang. Fabrication of reaction-bonded silicon carbide via phenolic/epoxy resin gelcasting [J]. Refractories, 2024, 58(4): 329-333. |
| [8] | Li Fei, Zhou Hui, Yang Zhichao, Tang Zhongdui, Wang Zhengfang, Liu Wei. Corrosion mechanism of working lining of refining ladle wall with different molding methods [J]. Refractories, 2024, 58(4): 344-348. |
| [9] | Li Kunpeng, Yan Shuangzhi, Zhang Tao, Shi Pengkun, Feng Zhiyuan, Fan Muxu, Wang Han, Liu Pengcheng. Corrosion of corundum mullite bricks by slag from rotary kilns [J]. Refractories, 2024, 58(4): 349-353. |
| [10] | Xu Xiaoying, Cao Haijie, Wei Lichao, Ma Xufeng. Application of energy dispersive X-ray fluorescence spectrometer in determination of magnesia composition [J]. Refractories, 2024, 58(4): 354-356. |
| [11] | You Jiegang, Zhao Xin, Qian Guohua, Zhang Xiao-fang, Zhang Guodong, Ma Beiyue. Development status of fused magnesia in southern Liaoning [J]. Refractories, 2024, 58(4): 357-361. |
| [12] | Tan Qitong, Zhao Huizhong, Yu Jun, Zhang Han, Tan Liqiang. Synthesis technology and properties of cordierite from solid waste resources [J]. Refractories, 2024, 58(3): 185-189. |
| [13] | Wang Xinyue, Xu Qing, Zhu Xinxin, Zhou Ruiqi, Duan Hongjuan, Zhang Haijun, Li Shaoping. Synthesis of porous MgAl2O4 fibers by solid-state reaction [J]. Refractories, 2024, 58(3): 190-194. |
| [14] | Cheng Xu, Deng Chengji, Dong Bo, Zou Qiliang, Ding Jun, Wang Zhoufu, Zhu Wanzheng, Xiao Yuyan, Zhu Hongxi, Yu Chao. Effect of Y2O3 on properties of oxide-bonded Ti(C,N) composites [J]. Refractories, 2024, 58(3): 195-198. |
| [15] | Liu Zhongfei, Wu Feng, Li Xinwei, Liang Xiaocheng, Luo Xudong, Qian Guohua. Corrosion mechanisms of CaO to MgAl2O4 materials and ZrO2-MgAl2O4 materials [J]. Refractories, 2024, 58(3): 199-203. |
| Viewed | ||||||
|
Full text |
|
|||||
|
Abstract |
|
|||||