Preparation of porous MgAl2O4 ceramics by dry pressing-solid phase reaction route

Piao Jiasi, Du Qing-yang, Bai Jiahai   

  1. First author's address: School of Materials Science and Engineering,Shandong University of Technology,Zibo 255049,Shandong,China
  • Received:2022-12-18 Published:2023-12-25

干压成型-固相反应法制备MgAl2O4多孔陶瓷

朴佳思1,2), 杜庆洋1), 白佳海1)   

  1. 1)山东理工大学 材料科学与工程学院 山东淄博 255049
    2)山东工业陶瓷研究设计院有限公司 山东淄博 255049
  • 通讯作者: 白佳海
  • 作者简介:朴佳思:女,1997年生,硕士研究生。E-mail:1597180588@qq.com
  • 基金资助:
    山东省自然科学基金资助项目(ZR2019MEM045)。

Abstract: To solve the problem of property decline caused by the volume expansion during the preparation of porous MgAl2O4 ceramics by solid phase sintering method,porous MgAl2O4 ceramics were prepared via the dry pressing-solid phase reaction route using Al2O3 (d50=1.1 μm) and MgO (d50=1.5 μm) as the main raw materials and TiO2 (d50=1.5 μm) as the additive.Influences of hot treatment temperatures (1 300,1 350,1 400,1 450,and 1 500 ℃) and TiO2 additions ( 0,0.5%,1.0%,1.5%,and 2.0%,by mass) on the linear change rate on heating,apparent porosity,bulk density,phase composition and microstructure of the porous MgAl2O4 ceramics were investigated.The experimental results show that:(1)as the hot treatment temperature increases,the densification of the porous ceramics increases,the bulk density increases but the apparent porosity decreases;(2)as the TiO2 addition increases,the linear shrinkage rate on heating of the porous ceramics increases,the apparent porosity decreases remarkably,while the average grain size increases.

Key words: porous MgAl2O4 ceramics, hot treatment temperature, TiO2, apparent porosity, microstructure

摘要: 为了解决固相烧结法制备MgAl2O4多孔陶瓷过程中体积膨胀导致性能下降的问题,以d50=1.1 μm的Al2O3和d50=1.5 μm的MgO为主要原料,d50=1.5 μm的TiO2为外加剂,用干压成型-固相反应法制备MgAl2O4多孔陶瓷。研究了热处理温度(1 300、1 350、1 400、1 450、1 500 ℃)和TiO2外加量(质量分数分别为0、0.5%、1.0%、1.5%、2.0%)对多孔陶瓷烧后线变化率、显气孔率、体积密度、物相组成和显微结构的影响。结果表明:1)随着热处理温度的升高, MgAl2O4多孔陶瓷的致密化程度提高,体积密度增大,显气孔率降低;2)随着TiO2外加量的增加,MgAl2O4多孔陶瓷的烧后线收缩率增大,显气孔率显著降低,平均晶粒尺寸增大。

关键词: MgAl2O4多孔陶瓷, 热处理温度, TiO2, 显气孔率, 显微结构