Refractories ›› 2025, Vol. 59 ›› Issue (2): 138-143.DOI: 10.3969/j.issn.1001-1935.2025.02.009

Previous Articles     Next Articles

Preparation and properties of novel yttria-silica enhanced zirconia composite aerogels

Li Zhanfeng, Sui Xue-ye, Tang Wenzhe, Liu Ruixiang, Wang Mengmeng   

  1. First author’s address:Shandong Industrial Ceramic Research and Design Institute Co.,Ltd.,Zibo 255000,Shandong,China
  • Received:2024-05-26 Online:2025-04-15 Published:2025-04-14

新型Y2O3-SiO2增强ZrO2复合气凝胶的制备及性能研究

李占峰, 隋学叶, 唐文哲, 刘瑞祥, 王蒙蒙   

  1. 山东工业陶瓷研究设计院有限公司 山东淄博 255000
  • 作者简介:李占峰:男,1996年生,硕士研究生,工程师。E-mail:17864197362@163.com

Abstract: The phase transition of ZrO2 at high temperatures causes structural collapse of ZrO2 aerogels.To improve the high-temperature stability of ZrO2 aerogels,Y2O3-SiO2 enhanced ZrO2 composite aerogels were prepared via the sol-gel method using low-cost and non-toxic mercaptosuccinic acid as a gel accelerator,and zirconium oxychloride octahydrate,yttrium nitrate hexahydrate,and tetraethyl orthosilicate as the precursors.Mullite fiber-Y2O3-SiO2-reinforced ZrO2 composites were also fabricated by adding mullite fibers.The effects of the molar ratios of Y2O3 to ZrO2 (1∶40,1∶20,1∶10,and 1∶5),SiO2 to ZrO2 (1∶10,1∶5,3∶10,and 2∶5) on the gel time,pore structure,and high-temperature properties were investigated.The results show that:Y2O3 and SiO2 can effectively shorten the gel time;SiO2 doping leads to a more uniform nanoporous structure;Y2O3 doping causes coarser skeletons and disordered nanopores;Y2O3 and SiO2 hinder the phase transition and reduce the shrinkage of ZrO2 at high temperatures.The optimal ratio of Y2O3-SiO2 enhanced ZrO2 composite aerogels was n(Y2O3)∶n(SiO2)∶n(ZrO2)=1∶3∶10.

Key words: ZrO2 aerogels, Y2O3, SiO2, thermal insulation

摘要: ZrO2在高温下的相变会引发ZrO2气凝胶的结构坍塌,为了提高ZrO2气凝胶的高温稳定性,以低成本、无毒的巯基琥珀酸为凝胶促进剂,八水氧氯化锆、六水硝酸钇、正硅酸乙酯为前驱体,采用溶胶-凝胶法制备了Y2O3-SiO2增强ZrO2复合气凝胶,并加入莫来石纤维,制备了莫来石纤维复合Y2O3-SiO2增强ZrO2材料,研究了Y2O3和ZrO2的物质的量比(分别为1∶40、1∶20、1∶10和1∶5)、SiO2和ZrO2的物质的量比(分别为1∶10、1∶5、3∶10 和2∶5)对ZrO2气凝胶的凝胶时间、孔结构以及高温性能的影响。结果表明:Y2O3和SiO2可有效缩短凝胶时间;掺入SiO2后,气凝胶的纳米孔结构更加均匀,但是掺入Y2O3后,气凝胶的骨架变粗,表现出杂乱的纳米孔结构;Y2O3和SiO2有效地阻碍了ZrO2的高温相变,降低了ZrO2的高温收缩率;制备Y2O3-SiO2增强ZrO2复合气凝胶的最佳配比为:n(Y2O3)∶n(SiO2)∶n(ZrO2)=1∶3∶10。

关键词: ZrO2气凝胶, Y2O3, SiO2, 隔热