Refractories ›› 2026, Vol. 60 ›› Issue (2): 179-184.DOI: 10.3969/j.issn.1001-1935.2026.02.017

Previous Articles    

Research progress on 3D printing technology for alumina ceramics

Yan Xiuxiu, Wang Yong, Cao Jiwei   

  1. First author’s address:Shared Intelligent Equipment Co.,Ltd.,Yinchuan 750021,Ningxia,China
  • Received:2025-04-03 Online:2026-04-15 Published:2026-04-15

氧化铝陶瓷3D打印技术研究进展

剡秀秀, 王勇, 曹继伟   

  1. 共享智能装备有限公司 宁夏银川 750021
  • 作者简介:剡秀秀:女,1997年生,硕士,工程师。E-mail:Maryam@163.com
  • 基金资助:
    宁夏回族自治区重点研发计划(2024BEE02009)。

Abstract: Alumina ceramics demonstrate significant application value across numerous fields due to their exceptional properties,such as high hardness,wear resistance,high-temperature resistance,chemical stability,electrical insulation,and biological inertness.This paper focused on the current research status of the binder jetting 3D printing technology,vat photopolymerization technology,selective laser sintering/melting technology,and fused deposition modeling technology in the fabrication of alumina ceramics.The advantages and disadvantages of each process were compared and analyzed.Finally,the development of 3D-printed alumina ceramics was prospected.

Key words: alumina, 3D printing, sintering additives, binders

摘要: 氧化铝陶瓷凭借硬度高、抗磨损、耐高温、化学稳定、电绝缘及生物惰性等优异性能,在众多领域展现出重要的应用价值。重点介绍黏结剂喷射3D打印技术、还原光聚合技术、选择性激光烧结/熔融技术、熔融沉积制造技术在氧化铝陶瓷制备中的研究现状,对比分析了各种工艺的优缺点,最后对3D打印氧化铝陶瓷的发展进行了展望。

关键词: 氧化铝, 3D打印, 烧结助剂, 黏结剂

CLC Number: