Effect of BF slag and desulfurized slag on corrosion resistance of Al 2O 3-SiC-C castables
Wen Taiyang, Cui Yuanyan, Zhong Kai, Yang Bin
Refractories . 2021, (2): 148 -150 .  DOI: 10.3969/j.issn.1001-1935.2021.02.013