Determination method of ferrous oxide content in hercynite
Xu Na, Liu Lanfang, Wu Feng, Li Xinwei, Luan Xu
Refractories . 2021, (
2
): 182 -184 . DOI: 10.3969/j.issn.1001-1935.2021.02.020