Preparation and machinability of nozzle plates for aluminum strip continuous casting and rolling
Wang Ziqiang, Wang Dongdong, Yang Min, Wang Gang, Huang Jiayuan, Zhou Huijun
Refractories . 2021, (3): 217 -220 .  DOI: 10.3969/j.issn.1001-1935.2021.03.008