Effect of electro-fused dense corundum and tabular alumina on structure and properties of corundum-mullite refractories
Hou Xiaojing, Li Zhigang, Zhang Zhenyan
Refractories . 2021, (3): 221 -225 .  DOI: 10.3969/j.issn.1001-1935.2021.03.009