Effect of repeated usage on thermal insulation properties of fiber reinforced SiO 2 aerogel materials
Tian Xiangyu, Han Yinlong, Zhou Liang, Wu Qiong, Shang Lei, Gao Qingfu, Zhang Bo
Refractories . 2021, (2): 116 -120 .  DOI: 10.3969/j.issn.1001-1935.2021.02.006