Influence of proportion of fly ash to Al(OH) 3 on preparation of porous mullite materials
Hu Qiguo, Liu Ying, Shao Qing, Li Ji
Refractories . 2021, (4): 302 -304 .  DOI: 10.3969/j.issn.1001-1935.2021.04.006