Effect of magnesium hydroxide particle size on structure and properties of corundum-spinel materials
Huang Chuan, Ni Yue’e, Ke Changming, Liu Xuexin, Wang Jingran, Zhang Jinhua
Refractories . 2021, (4): 305 -308 .  DOI: 10.3969/j.issn.1001-1935.2021.04.007