Effects of ZrO
2
on properties of corundum-cordierite-mullite composite phase materials prepared by sludge in aluminum profile plant
Luo Jinrong
Refractories . 2021, (
4
): 335 -337 . DOI: 10.3969/j.issn.1001-1935.2021.04.015