Research progress of bonding systems for Al
2
O
3
-C sliding plates
Yin Xin, Liu Zhenglong, Ding Jun, Yu Chao, Deng Chengji, Zhu Hongxi
Refractories . 2021, (
5
): 385 -389 . DOI: 10.3969/j.issn.1001-1935.2021.05.003