Combustion synthesis of C/MgAl 2O 4 composite powders and their microstructure evolution
Lyu Lihua, Ding Donghai, Xiao Guoqing
Refractories . 2021, (5): 405 -409 .  DOI: 10.3969/j.issn.1001-1935.2021.05.007