Effect of SiC content on structure and properties of SiC-Al composites fabricated by selective laser melting
Xie Houbo, Zhang Jialian, Yuan Gaoqian, Zhang Jingzhe, Li Kezhuo, Li Faliang, Zhang Haijun
Refractories . 2021, (
5