Effect of β-SiAlON content on properties of SiAlON bonded corundum materials
Liu Chenhui, Zhang Yucui, Jia Quanli, Ye Fangbao, Zhong Xiangchong
Refractories . 2021, (5): 452 -455 .  DOI: 10.3969/j.issn.1001-1935.2021.05.017