Effect of different calcium aluminate cements on properties of Al 2O 3-SiC-C iron trough castables
Niu Chunlin, Ren Lin, Zhang Xiaobo
Refractories . 2021, (6): 483 -486 .  DOI: 10.3969/j.issn.1001-1935.2021.06.005