Effect of holding time on phase composition and microstructure of SiC-TiC composite powder
Liu Xin, Hu Jilin, Zhu Ling, Tian Xiuying, Peng Yangxi
Refractories . 2021, (6): 487 -490 .  DOI: 10.3969/j.issn.1001-1935.2021.06.006