Optimization of pore structure and properties of porous Al
2
O
3
materials utilizing morphology of walnut shell
Hu Jiaojiao, Li Shujing, Li Yuanbing, Wei Zhipeng, Chen Pan, Wang Jianing
Refractories . 2022, (
1
): 10 -15 . DOI: 10.3969/j.issn.1001-1935.2022.01.003