Effect of oxidation temperature and dispersant type on properties of Si 3N 4 slurry
Sun Yijie, Ma Yan, Wang Zhoufu, Liu Hao, He Jian, Lyu Xusheng, Wang Xitang
Refractories . 2022, (1): 24 -28 .  DOI: 10.3969/j.issn.1001-1935.2022.01.006