Effect of adding cutting waste on preparation of silicon carbide from silica fume
Wang Bo, Zhou Tong, Ding Xu, Guo Zhicheng, Zhuang Yanxin, Gao Shuaibo, Xing Pengfei
Refractories . 2022, (1): 38 -42 .  DOI: 10.3969/j.issn.1001-1935.2022.01.009