中文
Finite element analysis on energy saving effect of lining materials of a 5.42 m
3
shuttle kiln body and their optimal configuration
Meng Chao, Wang Pengcan, Yang Wengang, Meng Qingxin, Xu Jiajia
Refractories . 2022, (
1
): 65 -70 . DOI: 10.3969/j.issn.1001-1935.2022.01.015