Effect of TiO
2
addition on properties of Al
2
O
3
ceramics prepared by digital light printing (DLP)
Wang Rui, Yang Daoyuan, Yuan Huiyu, Cui Junyan
Refractories . 2022, (
2
): 112 -116 . DOI: 10.3969/j.issn.1001-1935.2022.02.004