Preparation of magnesium aluminate spinel hollow sphere heat insulation refractories by foaming method
Ren Weili, Yang Daoyuan, Wang Rui, Jiang Qiao, Fu Yanxu, Liu Hao
Refractories . 2022, (
2
): 117 -122 . DOI: 10.3969/j.issn.1001-1935.2022.02.005