Phase reconstruction and microstructure evolution of magnesia-carbon refractories at high temperatures in nitrogen
Yan Mingwei, Yang Yumin, Tong Shanghao, Zhang Jiayu, Sun Guangchao, Liu Kaiqi
Refractories . 2022, (2): 93 -100 .  DOI: 10.3969/j.issn.1001-1935.2022.02.001