Effect of micro-sized calcium carbonate on hydration behavior of CAC at 20 ℃
Liu Mingyang, Wang Saixin, Ma Zhenyou, Jin Dongmei, Zhou Wenying, Mu Yuandong, Ye Guotian
Refractories . 2022, (3): 206 -209 .  DOI: 10.3969/j.issn.1001-1935.2022.03.006