Effect of particle size of Si 3N 4 powder on oscillatory pressure sintered Si 3N 4 ceramics
Xu Guangping, He Jiangrong, Liu Pengcheng, Mao Zhongjun, Qin Xiaowei, Xie Zhipeng
Refractories . 2022, (3): 214 -217 .  DOI: 10.3969/j.issn.1001-1935.2022.03.008