Microstructure analysis of α-Al 2O 3 prepared by aluminum hydroxide
Kang Dongdong, Feng Yu, Han Lu, Lu Zhiyan, Tang Bing, Cui Juan, Wu Feng
Refractories . 2022, (3): 218 -221 .  DOI: 10.3969/j.issn.1001-1935.2022.03.009