Optimizing production technique of forsterite lightweight spherical aggregates based on orthogonal design
Meng Qingxin, Yu Bingpo, Gao Lei, Chen Haojing, Xu Jiajia
Refractories . 2022, (
3
): 226 -230 . DOI: 10.3969/j.issn.1001-1935.2022.03.011