Entire hydrophobic modification of calcium aluminate cement products by polydimethylsiloxane
Li Bing, Zhang Haofeng, Guo Yusen, Hong Xumin, Dong Binbin, Yang Xiuli
Refractories . 2022, (3): 247 -250 .  DOI: 10.3969/j.issn.1001-1935.2022.03.015