Effect of Al powder and Si powder addition on structure and properties of unburned magnesium aluminate spinel refractories
Zhou Lianzhuo, Wang Zhoufu, Wang Xitang, Liu Hao, Ma Yan, Quan Zhenghuang
Refractories . 2022, (5): 380 -385 .  DOI: 10.3969/j.issn.1001-1935.2022.05.003