Effect of SiO
2
fume addition on thermal shock resistance of corundum castables
Li Yuchuan, Zhang Sanhua, Qin Hongbin, Chen Lu
Refractories . 2022, (
5
): 407 -411 . DOI: 10.3969/j.issn.1001-1935.2022.05.008