Effect of particle distribution on properties of corundum based dispersive purging plugs
Su Yuqing, Zhu Yening, Yu Baisong, Xi Zijian, Wei Juncong, Tu Junbo, Zhang Houxing, Wang Yilong
Refractories . 2022, (5): 427 -430 .  DOI: 10.3969/j.issn.1001-1935.2022.05.013