Sintering densification of boron carbide materials and their application research progress
Zou Xin, Chen Ping’an, Xu Guangping, Li Xiangcheng, Zhu Yingli, Zhu Boquan
Refractories . 2022, (5): 452 -457 .  DOI: 10.3969/j.issn.1001-1935.2022.05.018