Development of purging plugs for ladles and damaging mechanisms of typical composite structures
Chen Lu, Xu Yuanchao, Guo Peng, Zhang Hui, Wei Changsheng, Jia Qingwei
Refractories . 2022, (
4
): 283 -288 . DOI: 10.3969/j.issn.1001-1935.2022.04.002