Effect of ZrO 2 isolation layer on phase composition and microstructure of lanthanum aluminate high emissivity coating
Zhang Yifan, Wang Gang, Wang Qu, Zhang Qi, Wang Laiwen, Huang Zhenwu, Zhang Lei
Refractories . 2022, (4): 315 -319 .  DOI: 10.3969/j.issn.1001-1935.2022.04.009