Effect of B
4
C addition on properties of silica sol bonded mullite-corundum castables
Cai Wei, Chen Jinfeng, Ju Maoqi, Cong Peiyuan
Refractories . 2022, (
4
): 325 -328 . DOI: 10.3969/j.issn.1001-1935.2022.04.011