Effect of SiO 2 particle size and reaction temperature on synthesis of mullite whiskers by molten salt method
Su Yuxi, Li Xinwei, Wu Feng, Gao Yongjun, Luo Xudong, Feng Yu, Chen Weimin
Refractories . 2022, (4): 342 -345 .  DOI: 10.3969/j.issn.1001-1935.2022.04.015